01binary commented 7 years ago

"Make sure to melt the wax out completely at around 400 degrees then slowly bring it up to about 1000 - 1100 to completely bake the mold. "

01binary commented 7 years ago

Cracked at 80 F in a pre-heated oven (starting around 75 F).

01binary commented 7 years ago

http://scholarsmine.mst.edu/cgi/viewcontent.cgi?article=6002&context=masters_theses

01binary commented 7 years ago

http://webcache.googleusercontent.com/search?q=cache:hjov11owyfYJ:tomwade.me/tw/machinist/machinable-wax.pdf+&cd=2&hl=en&ct=clnk&gl=us

INVESTMENT CASTING Machinable Wax can be used for Investment Casting applications only if it can be flash fired out of the molds at a temperature of 1800 degrees F. The reason the high temperature is required is because the wax expands so much when going from a solid to a liquid that it will crack the ceramic shell unless it goes into that high temperature so quickly that the material will just disintegrate before this change occurs.